eFatigue gives you everything you need to perform state-of-the-art fatigue analysis over the web. Click here to learn more about eFatigue. GlossaryNeuber's RuleNeuber's rule is used to convert an elastically computed stress or stain into the real stress or strain when plastic deformation occurs. For example, we may compute a stress with elastic assumptions at a notch to be KtS and this stress exceeds the strength of the material. The real stress will be somewhere on the materials stress-strain curve at some point σ. ![]() Neuber's rule states, with some mathematical proof, that the product of the elastic solution is equal to the product of the real elastic plastic solution. Mathematically this is expressed as KtS⋅Kte=σ⋅ε. |
||