eFatigue gives you everything you need to perform state-of-the-art fatigue analysis over the web. Click here to learn more about eFatigue. GlossaryUltimate Strength (Su)The ultimate strength, Su, is also called the tensile strength. It is the maximum stress reached in an engineering stress strain diagram. ![]() |
||